MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® M77 Fast Curing Epoxy Resin Matrix
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: HexPly® M77 is a fast curing hotmelt, thermosetting epoxy resin matrix, specifically designed for prepreg applications at which short cure cycles are required. M77 is recommended for curing at 120 – 150°C and is suitable for a range of pressures (5 – 35bar). M77 can be used for manufacture of large industrial components, suitable for cure of thin and thick sections.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 - 1.25 g/cc0.0415 - 0.0452 lb/in³
Viscosity  4000 cP
@Temperature 115 °C
4000 cP
@Temperature 239 °F
5°C/min
 1.00e+8 cP
@Temperature 25.0 °C
1.00e+8 cP
@Temperature 77.0 °F
5°C/min
 1.00e+8 cP
@Temperature 136 °C
1.00e+8 cP
@Temperature 277 °F
5°C/min
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 125 - 135 °C257 - 275 °FOptimum cured, following a 2min cure @150°C
 125 - 135 °C257 - 275 °FTypical cured, following a 15min cure @130°C
 
Processing PropertiesMetricEnglishComments
Cure Time  <= 1.50 min
@Temperature 150 °C
<= 0.0250 hour
@Temperature 302 °F
time to 95% conversion; ISO 11357-5
 <= 3.00 min
@Temperature 140 °C
<= 0.0500 hour
@Temperature 284 °F
time to 95% conversion; ISO 11357-5
 <= 6.00 min
@Temperature 130 °C
<= 0.100 hour
@Temperature 266 °F
time to 95% conversion; ISO 11357-5
 <= 9.00 min
@Temperature 120 °C
<= 0.150 hour
@Temperature 248 °F
time to 95% conversion; ISO 11357-5
Shelf Life  1.50 Month
@Temperature 23.0 °C
1.50 Month
@Temperature 73.4 °F
 6.00 Month
@Temperature 5.00 °C
6.00 Month
@Temperature 41.0 °F
 18.0 Month
@Temperature -18.0 °C
18.0 Month
@Temperature -0.400 °F
 
Descriptive Properties
ColorOff white - Yellowish

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9152 / 322308

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.