3M™ Soft White Vinyl Label Product FV22902 is a flexible vinyl label stock that offers excellent durability and some moisture resistance. This vinyl label utilizes 3M™ Adhesive F2201 which is a freezer grade acrylic that offers high initial tack, good clarity, and adhesion when applied at temperatures as low as 0°F (-18°C) and also has excellent processing characteristics and offers exceptional adhesion to a wide variety of substrates with moderate resistance to water and humidity.Information provided by 3M |