MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Rogers Arlon 99-108065 PTFE Resin
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: Design/Construction:
Side 1: PTFE
Substrate: Style 1080 Fiberglass
Side 2: PTFE Resin

Appearance: Brown Woven Fabric

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 3.00 milOverall
Surface Tension <= 30 dynes/cmSurface Energy
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °F
Minimum Service Temperature, Air -40.0 °F
 
Processing PropertiesOriginal ValueComments
Shelf Life 60.0 Month
@Temperature 23.9 °C
From date of manufacture
 
Descriptive Properties
ColorBrown
Percent PTFE Resin Content35 % by Weight
Total Product Weight (oz/yd2).41Arlon SQA-TMS-025
Uncoated Fiberglass Break Strength70 x 40 lbs/inchArlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AGC Fluon® PTFE
Beijing Evergrow Resources PTFE Skived Sheet Tape
Mitsubishi Chemical Advanced Materials Fluorosint® 500 PTFE, synthetic mica-filled PTFE, compression molded (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Fluorosint® MT-01 Proprietary fluoropolymer reinforced with carbon fibers and organometallic fillers (ASTM Product Data Sheet)
DuPont Mobility and Materials Delrin® 100AF POM-PTFE20

PARL479 / 125665

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.