MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Michelman® Hydrosize® PA845H Polyamide dispersion
Categories: Fluid

Material Notes: ydrosize® PA845H can be applied via rod, air knife, gravure, spray and blade. Usage: Developed to be used as a carbon fiber sizing for high temperature applications, it also provides adhesion to various olefinic surfaces.

Applications (properties imparted): Cable & Cordage (adhesion promotion), Fiber Sizing (chopped strands, continuous fiber, thermal stability), Technical Textiles (adhesion promotion, binder, thermal stability).

Information provided by Michelman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 28 - 32 %28 - 32 %Non-Volatiles
pH 10 - 11.410 - 11.4
Brookfield Viscosity 0.00 - 500 cP0.00 - 500 cPSpindle #3. 60 RPM.
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 MonthDry, cool and well-ventilated place
 
Descriptive Properties
AppearanceWhite liquid
Emulsifier ChargeAnionic
Recommended pH> 7.0
Solids TypePolyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WMICHE9928 / 287523

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.