MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Matexcel GRA-390 GRA-390 Graphene powder, 1-5µm
Categories: Carbon

Material Notes: Graphene powder

Application: Energy storage and power batteries, new energy, solar energy, electronic components, printing, antistatic, electromagnetic shielding, high-performance coatings, lightweight and high-strength composite materials.

Morphology: Grey-black with slight metallic color

Key Words: Synonyms: GRA-390 Graphene powder, 1-5µm
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 1.0 - 5.0 µm
 
Descriptive Properties
Product overviewAsh (wt%): =1.00 Oxygen content (wt%): =0.01 Layers: =10 Powder resistivity (?/O·m): =1.0 x 10-3 Thermal conductivity (W/m·k): 6 (Perpendicular to the graphene surface); 3,000 (Parallel to graphene surface) Thermal expansion coefficient (1/K): (0.5-1.0)x10-6 (Perpendicular to the graphene surface); (4-6)x10-6 (Parallel to graphene surface)
Purity=99.00%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMXCK1415 / 300046

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.