MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 6042-60A MD Specialty Thermoplastic Elastomer; ISO 10993 Tested
Categories: Polymer; Thermoplastic; Elastomer, TPE

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccASTM D 792
Linear Mold Shrinkage 0.0080 - 0.016 cm/cm
@Thickness 3.20 mm
0.0080 - 0.016 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 606010 s delay; ASTM D 2240
Tensile Strength at Break  3.45 MPa
@Thickness 3.20 mm
500 psi
@Thickness 0.126 in
Die C; 20 in/min (500 mm/min); ASTM D 638
 8.27 MPa
@Thickness 3.20 mm
1200 psi
@Thickness 0.126 in
Break; Die C; 20 in/min (500 mm/min); ASTM D 412
50% Modulus 1.52 MPa
@Strain 50 %,
Thickness 3.20 mm
1.52 MPa
@Strain 50 %,
Thickness 0.126 in
Die C; 20 in/min (500 mm/min); ASTM D 412
100% Modulus 2.00 MPa
@Strain 100 %,
Thickness 3.20 mm
290 psi
@Strain 100 %,
Thickness 0.126 in
Die C; 20 in/min (500 mm/min); ASTM D 412
300% Modulus 3.93 MPa
@Strain 300 %,
Thickness 3.20 mm
570 psi
@Strain 300 %,
Thickness 0.126 in
Die C; 20 in/min (500 mm/min); ASTM D 412
Tear Strength 33.3 kN/m190 pliDie C; ASTM D 624
Compression Set  20 %
@Temperature 23.0 °C,
Time 79200 sec
20 %
@Temperature 73.4 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
 75 %
@Temperature 70.0 °C,
Time 79200 sec
75 %
@Temperature 158 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
 
Processing PropertiesMetricEnglishComments
Melt Temperature 193 - 238 °C380 - 460 °F
Mold Temperature 21.1 - 48.9 °C70.0 - 120 °F
Drying Temperature 82.2 °C
@Time 7200 - 14400 sec
180 °F
@Time 2.00 - 4.00 hour
Moisture Content <= 0.030 %<= 0.030 %
Dew Point <= -17.8 °C<= 0.000 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PQZUA21304 / 134779

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.