MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Materion ToughMet® 3 TS105 Copper-Nickel-Tin Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: ToughMet copper-nickel-tin alloys are engineered to provide attributes beyond those typically found in high-strength copper alloys, especially in the high temperature, high pressure regime. ToughMet materials retain their strength at elevated temperatures and resist most sour environments. Some ToughMet alloy tempers combine high levels of fracture toughness with strength. In addition to rod, bar, sheet and plate, ToughMet alloys are also offered in large diameter bar form, which offers very consistent properties throughout cross sections of the material in diameters more than double regular ToughMet alloy size ranges.

Advantages

  • High fatigue strength
  • Lower friction
  • Non-magnetic
  • Anti-galling
  • Corrosion, erosion and wear resistance
  • Resiliency
  • Excellent machinability

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 9.00 g/cc0.325 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 22.022.0
Tensile Strength 827 MPa120000 psi
Tensile Strength, Yield 724 MPa105000 psi
Elongation at Break 15.0 %
@Thickness 50.8 mm
15.0 %
@Thickness 2.00 in
Modulus of Elasticity 145 GPa21000 ksi
Poissons Ratio 0.3200.320
 
Electrical PropertiesMetricEnglishComments
Magnetic Permeability <= 1.001<= 1.001
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 38.0 W/m-K264 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NBB92234 / 323592

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.