MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Ixef® FC-1032 Polyarylamide (PARA), 60% glass fiber
Categories: Polymer; Thermoplastic; Polyarylamide (PAA); Polyarylamide, Glass Fiber Filled

Material Notes: 60% glass fiber, FDA-approved for food contact

Ixef® FC-1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.

Ixef® FC-1032 meets FDA regulations for Ixef® FC-1032 NT 000 (natural) and Ixef® FC-1032 BK 001 (black) based on clearances granted by FCN 001242 for repeated use food contact applications with all food types, under FDA conditions of use B through H as described in Tables 1 and 2 of 21 CFR 176.170(c).

Ixef® FC-1032 is also cleared for food contact use by European Union regulations.

- Black: FC-1032 BK 001
- Natural: FC-1032 NT 000

Applications: Appliances; Food Service Applications; High Gloss Applications; Hospital Goods

Features: Chemical Resistant; Creep Resistant; Food Contact Acceptable; General Purpose; Good Dimensional Stability; Good Sterilizability; High Flow; High Strength; Low Moisture Absorption; Outstanding Surface Finish; Ultra High Stiffness

Injection notes: Hot runners: 250°C to 260°C (482°C to 500°F)
Storage
Ixef® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Ixef® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Ixef® processing guide.
Drying
The material as supplied is ready for molding without drying. However, If the bags have been open for longer than 24 hours, the material needs to be dried. When using a desiccant air dryer with dew point of -28°C (-18°F) or lower, these guidelines can be followed: 0.5-1.5 hour at 120°C (248°F), 1-3 hours at 100°C (212°F), or 1-7 hours at 80°C (176°F).
Injection Molding
Ixef® FC-1032 compound can be readily injection molded in most screw injection molding machines. A general purpose screw is recommended, with minimum back pressure.
The measured melt temperature should be about 280°C (536°F), and the barrel temperatures should be around 250 to 260°C (482 to 500°F) in the rear zone, gradually increasing to 260 to 290°C (500 to 554°F) in the front zone. If hot runners are used, they should be set to 250 to 260°C (482 to 500°F).
To maximize crystallinity, the temperature of the mold cavity surface must be held between 120 and 140°C (248 and 284°F). Molding at lower temperatures will produce articles that may warp, have poor surface appearance, and have a greater tendency to creep. Set injection pressure to give rapid injection. Adjust holding pressure and hold time to maximize part weight. Transfer from injection to hold pressure at the screw position just before the part is completely filled (95-99%).

Information provided by Solvay Specialty Polymers.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.77 g/ccISO 1183
Water Absorption 0.13 %
@Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 280 MPaISO 527-2
Elongation at Break 1.8 %ISO 527-2
Tensile Modulus 24000 MPaISO 527-2
Flexural Strength 400 MPaISO 178
Flexural Modulus 23500 MPaISO 178
Izod Impact, Notched 120 J/mASTM D256
Izod Impact, Unnotched 900 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 14.0 µm/m-°CISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 230 °CUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 250 - 260 °C
Front Barrel Temperature 260 - 290 °C
Nozzle Temperature 260 - 290 °C
Melt Temperature 280 °CInjection
Mold Temperature 120 - 140 °C
Drying Temperature 120 °C
@Time 1800 - 5400 sec
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack; Natural Color
FormsPellets
Injection RateFast
ProcessingInjection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4294 / 280094

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.