- NEAM GPO-1
- Extremely Cost-Effective
- Outstanding Punchability
- Ideal For a Variety of Applications
- UL® Recognized
- Easily Fabricated
- Asbestos-Free
Grade TSF 1312 General-Purpose Laminate is the most cost-effective fiberglass-reinforced laminate sheet available from Rochling Glastic Composites. It is also NEMA GPO-1 Laminate and UL Recognized. Grade TSF 1312 has a UL temperature index of 130°C Electrical and 130°C Mechanical. It is available in the color brown, in thicknesses of 1/32 of an inch through 1 ¼ inches. Grade TSF 1312 exhibits outstanding punchability in thing thicknesses. It is widely used in motors and dry-type transformers, as well as a variety of other applications.Information provided by Röchling. |