MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt F 206 LF Putty
Categories: Polymer; Thermoset

Material Notes: F 206 series are low density fairing compound formulated for repair of FRP components. This compound can be used to make or modify plugs and molds. It is easy to sand and use and does not gum up sand paper and has a hard finish after a complete cure.

Features And Benefits:

  • F 206 is easily applied by using an appropriate tool such as spatula or a trowel.
  • Formulated to use with a MEKP catalyst made of methyl ethyl ketone peroxide.
  • This compound has low shrinkage (less than 1%) and has non-sagging properties.
  • Offers good impact and crack resistance
  • Good adhesion on polyesters and vinyl ester laminates and good water resistance.
  • F206LM contains a color indicator to ensure proper catalyst mix
  • Available in 20 liters pails and 205 liters drums

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.650 - 0.750 g/cc0.0235 - 0.0271 lb/in³
Brookfield Viscosity 100000 - 200000 cP100000 - 200000 cPT-D @ 10 rpm
 
Processing PropertiesMetricEnglishComments
Gel Time 3.00 - 6.00 min
@Temperature 18.0 °C
3.00 - 6.00 min
@Temperature 64.4 °F
use 1,25% Norox MEKP-9
Shelf Life 1.25 Month
@Temperature 18.0 °C
1.25 Month
@Temperature 64.4 °F
 
Descriptive Properties
Thixotropic Index>61/10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9014 / 231609

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.