MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Polyoil 130 Polybutadiene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Polyoil 130 is a nonpolar stereospecific, low viscosity, unsaponifiable liquid polybutadiene with a higher molecular weight than Polyoil 110. General uses include a plasticizer in rubber compounds, mold release agent for PUR foams, modification of resins, improvement in the air drying properties of vegetable oils, sole binder for single-layer surface coatings for interior use, and a binder for recycled rubber compounds.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 - 0.920 g/cc
@Temperature 20.0 °C
DIN 51 757
Iodine Absorption Number 420 - 480g of Iod/ 100g; DIN 53 241
Viscosity 2700 - 3300 cP
@Temperature 20.0 °C
DIN EN ISO 3219
Molecular Weight 3000 g/molVapor Pressure Osmometry
 3800 g/molGPC
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.30DIN EN ISO 2114
 
Thermal PropertiesOriginal ValueComments
Pour Point -50.0 °CDIN ISO 3016
Flash Point 200 °CDIN EN ISO 2719
Ignition Temperature 350 °CDIN 51 794
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 4.0DIN ISO 4630
 
Descriptive Properties
Peroxide Number (mval/kg)<10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polybutadiene Rubber (BR)
ChevronTexaco Texatherm®
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride
Solvay Chemicals SOLKANE® 143a
Unipetrol Normal 91 Unleaded MOGAS

PHUMB339 / 81341

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.