MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm XT® Polymer 250 Clear/ natural Acrylic-Based Multipolymer Compound
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes: XT polymer 250 compound is an impact-modified acrylic-based multipolymer for molding, extrusion and blow molding applications. Typical properties of XT polymer 250 compound are:
  • outstanding thermoformability
  • superior heat distortion temperatures
  • excellent bonding and welding capabilities
  • good impact strength
  • good light transmission
  • resistant to EtO, gamma and E-beam sterilization
  • resistant to PVC plasticizers
The special property of XT polymer 250 compound is
  • high strength properties
  • good chemical resistance
Application: Used for medical devices, food packaging, pharmaceutical packaging, rigid medical device packaging and appliance parts.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D792
Bulk Density 0.650 g/ccASTM D1895
Water Absorption <= 0.30 %ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D951
Melt Flow 4.2 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 56ASTM D785
Tensile Strength at Break 8000 psiASTM D638
Elongation at Break 15 %ASTM D638
Elongation at Yield 3.6 %ASTM D638
Tensile Modulus 430 ksiASTM D638
Flexural Strength 13000 psiASTM D790
Flexural Modulus 400 ksiASTM D790
Izod Impact, Notched 1.20 ft-lb/in
@Diameter 6.35 mm
BAR; ASTM D256
 0.900 ft-lb/in
@Diameter 6.35 mm,
Temperature 0.000 °C
BAR; ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 µin/in-°F
@Temperature 0.000 - 100 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 189 °F
@Thickness 6.35 mm
Annealed; ASTM D648
Vicat Softening Point 214 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.51ASTM D542
Haze 2.5 %ASTM D1003
Yellow Index 4.0 %ASTM E313
Transmission, Visible 90 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 400 - 475 °FCylinder Temp
Melt Temperature 400 - 475 °F
Mold Temperature 120 - 170 °F
Drying Temperature 180 °F
Dry Time 3 - 4 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Terluran® GP-35 ABS
Fainplast Compounds MRT 256/G Medical Rigid PVC, Injection Molding
Röhm XT® Polymer 250 Clear/ Blue Tint Acrylic-Based Multipolymer Compound
Axiall 9175 White 10 Rigid PVC, Molding, White 10
Axiall 6511 Rigid PVC, Molding

PCYR00037 / 89041

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.