MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ELM® SoyGrease™ EP Plus Biodegradable Extreme Pressure Grease, NLGI Grade 3
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Description: ELM SoyGrease™ EP Plus grease is a premium quality biodegradable, Biotechbased™ grease formulated with OptiBase™ Oils, lithium-based thickener and extreme pressure additives for maximum performance.

Applications:

  • Recommended for fleet, farm, household and industrial applications
  • Suitable as Fifth Wheel Grease
  • Ideal for heavy load applications
  • Engineered for off-highway equipment
  • Designed for extreme pressure applications
  • Recommended for environmentally sensitive areas near waterways
Benefits:
  • Extreme pressure additives minimize friction and wear
  • Biodegradable formula is friendly to the environment
  • High film strength of vegetable oil provides superior lubricity
  • Excellent oxidative and high-temperature stability
  • Higher flash point than petroleum greases for increased safety
  • Meets EPA’s Environmental Preferable Purchasing (EPP) criteria
  • Meets USDA’s proposed Biobased product definition for EO 13101
  • Manufactured from renewable USA-grown crop base oils
  • Complies with State of Iowa SF 2249 – Purchasing Preference for Biobased Lubricants

Information provided by ELM®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Kinematic Viscosity at 40°C (104°F) 86 cSt
Kinematic Viscosity at 100°C (212°F) 16 cSt
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 600 kg
Four Ball Wear 0.500 mm
Penetration 220 - 250Cone, worked 60 strokes
 
Thermal PropertiesOriginal ValueComments
Flash Point 326 °CBase Oil
 
Descriptive Properties
AppearanceRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ELM® SoyGrease™ HiTemp Biodegradable Extreme Pressure Grease, NLGI Grade 3
ELM® SoyGrease™ EP Premium Biodegradable Extreme Pressure Grease, NLGI Grade 2
ELM® SoyGrease™ EP Plus Biodegradable Extreme Pressure Grease, NLGI Grade 2
ELM® SoyGrease™ Biodegradable Grease for Semi-Truck Fifth Wheels
Cossa Polimeri ESTABIO EX 03120 B Biodegradable Plastic, Calcium Carbonate Filled

WELML006 / 146209

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.