MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ChevronTexaco Havoline® SAE 10W-30 Synthetic Blend Motor Oil
Categories: Fluid; Lubricant

Material Notes: Havoline Synthetic Blend Motor Oil is formulated with a combination of synthetic and premium quality conventional base oils and an advanced additive package.

Havoline Synthetic Blend Motor Oil is recommended for all four-stroke gasoline engines used in passenger cars, light trucks, powerboats, motorcycles, and other mobile and stationary equipment. It is excellent for high-revving engines in small cars and light trucks. It was specially formulated for use in turbocharged engines. It meets:

  • API Service Categories SL, SJ, SH, SG, Energy conserving for API SL
  • ILSAC GF-3
  • Ford ESE-M2C 153-G
  • General Motors GM 6094M
  • Department of Defense Commercial Item Description A-A-52306
  • USDA H2

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 222105; MSDS Number: 8601

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 30.2 °
Viscosity 6400 cP
@Temperature -25.0 °C
Cold Crank
Viscosity Measurement 134Viscosity Index
Kinematic Viscosity at 40°C (104°F) 76 cSt
Kinematic Viscosity at 100°C (212°F) 11 cSt
Ash 0.90 %Sulfated Ash
 
Chemical PropertiesOriginal ValueComments
Total Base Number 8.2ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -39.0 °C
Flash Point 234 °C
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 0.098 %
Zinc, Zn 0.109 %
 
Descriptive Properties
Noack Volatility, wt%10.5250°C, 1 h

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WTEXA086 / 76965

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.