MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cast Nylons Nycast® 6PA-MoS2 Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: NYCAST® 6PA-MoS2 is a molybdenum disulphide filled Type 6 cast nylon. Finely divided MoS2 particles are suspended in the melt during polymerization. This gives the NYCAST® 6PA-MoS2 products improved compression strength over the regular Nycast 6PA products.

Data provided by the manufacturer, Cast Nylons Limited.

The data below are average values presented for comparison purposes. Actual property values may differ.

Key Words: Polyamide 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccASTM D792
Water Absorption 0.50 %24 hrs; ASTM D570
Water Absorption at Saturation 5.5 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Hardness, Shore D 80ASTM D2240
Tensile Strength, Ultimate 88.0 MPaASTM D638
Elongation at Break 20 - 45 %ASTM D638
Tensile Modulus 3.60 GPaASTM D638
Flexural Yield Strength 114 MPaASTM D790
Flexural Modulus 3.20 GPaASTM D790
Compressive Yield Strength 114 MPa10% Offset; ASTM D695
Compressive Modulus 2.20 GPaASTM D695
Shear Strength 72.0 MPaASTM D732
Izod Impact, Notched 0.400 J/cmASTM D256
Coefficient of Friction, Dynamic 0.22
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.7
@Frequency 60 Hz
 3.7
@Frequency 1000 Hz
 3.7
@Frequency 100000 Hz
ASTM D150
Dielectric Strength 22.0 kV/mmShort time; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Melting Point 226 - 238 °CASTM D789
Maximum Service Temperature, Air 110 °CContinuous service
 166 °CIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 204 - 221 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 166 - 204 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger Tecamid® GF30 Extruded Nylon 6/6 30% glass-fiber-reinforced (PA66)
Cast Nylons Nycast® 6PA-Blue Nylon 6
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled
Cast Nylons Nycast® Nyloil® Lubricated Nylon
Cast Nylons Nycast® SLX Premium Bearing Grade Nylon

PCAST5 / 27942

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.