MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NYC YT3WBQ Y2O3 CIP (Cold Isostatic Pressing) Granules
Categories: Ceramic; Oxide

Material Notes: 99.9% and better high purity granules produce high quality finished ceramics. Uses include semiconductors / LCD industries, metallurgy, magnets, and electroceramics.
  • Acrylic binder system
  • Excellent green properties
  • Easy sintering with stable, low shrinkage rates

Key Words: Y2O3, Yttria, Yttrium Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 1.30 g/ccApparent Density of Granules
 1.40 g/ccTap Density of Granules
Porosity <= 2.0 %after sintering at 1650°C for 2 hours in air
Particle Size 0.50 µmRaw Material; Average; D50; Microtrac HRA
 40 µmGranules; Average; D50; Microtrac HRA
Specific Surface Area 6.0 m²/gRaw material; BET
 
Thermal PropertiesOriginal ValueComments
Shrinkage 20 %
@Temperature 1650 °C,
Time 7200 sec
 
Component Elements PropertiesOriginal ValueComments
Fe2O3 <= 0.0010 %ICP-AES
Na2O <= 0.0010 %AA
Y2O3 >= 99.9 %TREO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
H.C. Starck Amperit® 849.054 Sintered Yttria (Y2O3)
H.C. Starck Amperit® 847.6 Agglomerated Yttria (Y2O3)
Yttrium Oxide, Y2O3
MarkeTech Repton 922 Yttria Y2O3
MarkeTech Repton 314 Mullite

CNYC990 / 125938

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.