Hifax polypropylene resins based on the Catalloy process are used in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable), and automotive industries. Hifax priovides good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion. Hifax HSBM CB 1158 G G12435 is a 12% talc filled PP copolymer, with high melt flow and high impact resistance. Product is available as a customized color matched, pellet form. This grade is not intended for medical, pharmaceutical, food or drinking water applications. This grade is delivered in G12435 color version. Avoid prolonged storage in open sunlight. Storage at high temperatures (> 50°C) and high humidity may bring to loss of quality of the packaging and the material. Information provided by LyondellBasell. |