MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bostik Webpatch® 90 Gypsum Patch
Categories: Other Engineering Material

Material Notes: Description: Bostik Webpatch® 90 is a fast-setting, gypsum-based material designed for interior installations and may be used to patch floors, walls and other surfaces. Floor covering can be installed after just 1 hour from patch application. Bostik Webpatch 90 may be used to fill up to 1/2” deep over properly prepared concrete, masonry, cementitious backer board and structurally sound exterior grade plywood (interior/dry use only). When used properly, this product provides a fast-setting surface that will not check, crack or break up. The Webpatch 90 may be mixed with Bostik 425™ Multi-Purpose Acrylic Latex Admixture instead of water for improved performance.

Information provided by Bostik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Cure Time 20.0 - 30.0 minFinal Set
 672 hourFinal
Pot Life 10.0 - 20.0 min
Working Life 10.0 - 20.0 min
Shelf Life 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Gypsum (CaSO4 - 2H2O)
Calcium Hydroxyapatite, Ca10(PO4)6(OH)2
Bostik Webpatch® D-9001 Latex-Fortified Gypsum Patch

PBOSTK054 / 191590

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.