MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Michelman® HydraBan® 1000AF Water resistant paper coating
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Water resistant paper coating

Usage: HydraBan® 1000AF is an economical water based treatment for kraft paper. It imparts a high degree of water repellency, is printable and gluable.

Application data: HydraBan® 1000AF can be applied using a blade or rod coater, at the wet end of the corrugator, dry end of the corrugator or with an off-line operations. It is also sprayable.

HydraBan® is typically used for: Produce boxes; Outdoor storage and Home improvement product

Food Contact Information when manufactured in the USA and Belgium:
FDA:
175.105: Components of adhesives.
176.170: Components of paper and paperboard in contact with aqueous and fatty foods
176.180: Components of paper and paperboard in contact with dry foods.

When manufactured in Belgium product meets food contact regulations for:
Europe: Euro. Res. AP(2004)1(Restricted)
Germany: BfR Recommendation XIV (Restricted) and BfR Recommendation XXXVI (Restricted)

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 - 0.970 g/cc
pH 9.5 - 11
Brookfield Viscosity <= 50 cPSpindle # 1, rpm 60
Viscosity Measurement 13 - 23[sec], EZ cup, Cup # 2
 
Descriptive Properties
AppearanceWhite, low viscosity liquid
Solids TypeScale

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unifrax Isofrax® 1260C Paper Fiber
UBE Tyrannohex® Heat Resistant Composite
RheTech Products HP531-680UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, BJAA Light Parchment
RheTech Products G20P100-599 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford BJ4A) Medium Dark Parchment
Plastic Lumber from the Plastic Lumber Co.

WMICHEL022 / 134939

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.