MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow 3-4118 GEL A&B
Categories: Polymer; Thermoset; Silicone

Material Notes: Former Dow Corning product.

Information provided by Dow Corning

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/cc
@Temperature 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Penetration P(0), 1/10 mm 105
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.60e+15 ohm-cm
Dielectric Strength 450 V/mil
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -45.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 60.0 min
@Temperature 120 °C
Shelf Life 12.0 Month
 
Descriptive Properties
Appearanceclear
Flowableyes
Gel Hardness (Grams/Penetration)50
Hydrophobicyes
Self Levelingyes
Water Resistantyes
Working Time (min)30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow 3-6635 DIELECTRIC GEL
Parker Chomerics THERM-A-GAP™ GEL T630 Dispensable, Very Low Compression Force, Thermal Gap Filler
Parker Chomerics THERM-A-GAP™ A174 Highly Conformable, Thermally Conductive Gap Filler
NuSil GEL-8100 Silicone Gel
Lord Adhesives Gelease™ MG-200 Thermally Conductive Silicone Gel Interface

PDOWCO323 / 106024

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.