MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

SABIC NORYL™ Resin EN185 Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ EN185 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This extrusion grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of v0 at 3mm and V1 at 1.5mm. NORYL EN185 resin exhibits excellent impact strength, very low moisture absorption, good dimensional stability, and great machinability. NORYL EN185 resin is an excellent candidate for a variety of applications including fiber optic ducting,

Features: Hydrolytic Stability,Flame Retardant,Good Stiffness,Non-Halogenated,Non-Chlorinated,High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D792
Water Absorption 0.070 %
@Time 86400 sec
0.070 %
@Time 24.0 hour
ASTM D570
Moisture Absorption 0.0200 %0.0200 %Extrusion
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 113113ASTM D785
Tensile Strength, Yield 42.0 MPa6090 psi50 mm/min; ASTM D638
Elongation at Break 50 %50 %50 mm/min; ASTM D638
Flexural Strength 67.0 MPa9720 psiyld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 2.27 GPa329 ksi2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 389 J287 ft-lbASTM D256
 160 J
@Temperature -40.0 °C
118 ft-lb
@Temperature -40.0 °F
ASTM D256
Gardner Impact  13.0 J
@Temperature -40.0 °C
9.59 ft-lb
@Temperature -40.0 °F
ASTM D3029
 24.0 J
@Temperature -30.0 °C
17.7 ft-lb
@Temperature -22.0 °F
ASTM D3029
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.8
@Frequency 50.0 - 60.0 Hz
2.8
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 24.8 kV/mm
@Thickness 3.20 mm
630 kV/in
@Thickness 0.126 in
in oil; ASTM D149
Dissipation Factor  0.0035
@Frequency 1e+6 Hz
0.0035
@Frequency 1e+6 Hz
IEC 60250
 0.0040
@Frequency 50.0 - 60.0 Hz
0.0040
@Frequency 50.0 - 60.0 Hz
ASTM D150
Arc Resistance 0.00 - 60 sec0.00 - 60 secASTM D495
Comparative Tracking Index 250 - 400 V250 - 400 VUL 746A
Hot Wire Ignition, HWI  30 - 60 sec
@Thickness >=1.50 mm
30 - 60 sec
@Thickness >=0.0591 in
UL 746A
 60 - 120 sec
@Thickness >=3.00 mm
60 - 120 sec
@Thickness >=0.118 in
UL 746A
 >= 120 sec
@Thickness >=6.00 mm
>= 120 sec
@Thickness >=0.236 in
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=1.50 mm
>= 120 arcs
@Thickness >=0.0591 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min>= 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 73.8 µm/m-°C
@Temperature -40.0 - 95.0 °C
41.0 µin/in-°F
@Temperature -40.0 - 203 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
@Thickness 6.40 mm
199 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
@Thickness 6.40 mm
180 °F
@Thickness 0.252 in
unannealed; ASTM D648
Flammability, UL94  V-1
@Thickness >=1.50 mm
V-1
@Thickness >=0.0591 in
UL 94
 V-0
@Thickness >=3.00 mm
V-0
@Thickness >=0.118 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 1 170 °C338 °FExtrusion
Zone 2 170 °C338 °FExtrusion
Zone 3 190 °C374 °FExtrusion
Zone 4 190 °C374 °FExtrusion
Adapter Temperature 205 °C401 °FExtrusion
Die Temperature 205 °C401 °FExtrusion
Melt Temperature 195 - 210 °C383 - 410 °FExtrusion
Drying Temperature 90.0 - 100 °C194 - 212 °FExtrusion
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourExtrusion
 8.00 hour8.00 hourCumulative; Extrusion
 
Descriptive Properties
Radiant Panel ListingTRUEUL Tested

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82278 / 290225

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.