MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150 (Heated 621°C)
Categories: Metal; Ferrous Metal; Stainless Steel; Precipitation Hardening Stainless; T S10000 Series Stainless Steel

Material Notes: Data provided by Carpenter Technology Corporation.

Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosion resistance. It has good fabricating characteristics and can be age hardened by a single-step, low temperature treatment. It has been used for a variety of applications including oil field valve parts, chemical process equipment, aircraft fittings, fasteners, pump shafts, nuclear reactor components, gears, paper mill equipment, missile fittings, and jet engine parts. Project 70® stainless Custom 630 is an improved machinability modification.

Key Words: AISI 630; UNS S17400; 17-4PH, 17/4PH, 17-4 PH, Precipitation Hardening PH Stainless Steel, 17-4
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.82 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 311
Hardness, Knoop 337Estimated from Rockwell C
Hardness, Rockwell C 33
Hardness, Vickers 325Estimated from Rockwell C
Tensile Strength, Ultimate 993 MPa
Tensile Strength, Yield 869 MPa
@Strain 0.2 %
Elongation at Break 20 %
Reduction of Area 60 %
Modulus of Elasticity 197 GPaH900 Condition
Poissons Ratio 0.272
Shear Modulus 77.4 GPaCalculated
Charpy Impact 75.0 JV-notch
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000770 ohm-cmfor condition H 900
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.9 µm/m-°C
@Temperature 21.0 - 93.0 °C
 12.8 µm/m-°C
@Temperature 21.0 - 316 °C
 13.0 µm/m-°C
@Temperature 21.0 - 427 °C
Specific Heat Capacity 0.419 J/g-°C
@Temperature 0.000 - 100 °C
condition H 900
Thermal Conductivity 17.9 W/m-K
@Temperature 149 °C
condition H 900
 22.6 W/m-K
@Temperature 482 °C
condition H 900
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.070 %
Chromium, Cr 15 - 17.5 %
Copper, Cu 3.0 - 5.0 %
Iron, Fe 73 %as remainder
Manganese, Mn <= 1.0 %
Nb + Ta 0.15 - 0.45 %
Nickel, Ni 3.0 - 5.0 %
Niobium, Nb (Columbium, Cb) <= 0.45 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %
Tantalum, Ta <= 0.45 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Annealed
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1025 (Heated 552°C)
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150M (Heated 760°C/2hr/AC then 621°C/4hr/AC)
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 900 (Age-Hardened 482°C/1hr/AC)
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1075 (Heated 579°C)

NCARH3 / 15770

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.