Luran® S KR2864C is a blend of ASA and PC offering high heat resistance, good impact strength and enhanced flowability. High flowability, High heat resistance, High impact strength. Applications: Truck fenders, Truck cabin parts, Truck body panels. Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |