MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Alcohol (EVOH)

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 - 1.24 g/ccAverage value: 1.17 g/cc Grade Count:43
Moisture Absorption at Equilibrium 1.50 - 8.50 %Average value: 3.86 % Grade Count:7
Moisture Vapor Transmission 0.360 - 3.10 cc-mm/m²-24hr-atmAverage value: 1.13 cc-mm/m²-24hr-atm Grade Count:26
Water Vapor Transmission 14.28 - 217.1 g/m²/day
@Temperature 37.8 - 37.8 °C
Average value: 126 g/m²/day Grade Count:3
Oxygen Transmission 0.00400 - 0.0640 cc-mm/m²-24hr-atmAverage value: 0.0179 cc-mm/m²-24hr-atm Grade Count:39
Oxygen Transmission Rate 0.310 - 1.55 cc/m²/dayAverage value: 1.08 cc/m²/day Grade Count:4
Viscosity 170000 - 1.40e+7 cP
@Temperature 200 - 230 °C
Average value: 1.81e+6 cP Grade Count:11
 170000 - 1.40e+7 cP
@Shear Rate 60.0 - 270 1/s
Average value: 1.81e+6 cP Grade Count:11
Thickness 15.2 - 63.5 micronsAverage value: 32.0 microns Grade Count:6
Melt Flow 0.800 - 22.0 g/10 minAverage value: 5.46 g/10 min Grade Count:38
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 85.0 - 104Average value: 94.0 Grade Count:12
Tensile Strength, Ultimate 37.0 - 74.0 MPaAverage value: 57.3 MPa Grade Count:3
Tensile Strength, Yield 43.0 - 94.0 MPaAverage value: 66.8 MPa Grade Count:12
Film Elongation at Break, MD 70.0 - 390 %Average value: 238 % Grade Count:16
Film Elongation at Break, TD 85.0 - 390 %Average value: 237 % Grade Count:7
Elongation at Break 130 - 330 %Average value: 233 % Grade Count:3
Elongation at Yield 1.00 - 8.00 %Average value: 5.14 % Grade Count:7
Modulus of Elasticity 1.08 - 3.10 GPaAverage value: 2.16 GPa Grade Count:13
Flexural Yield Strength 108 - 150 MPaAverage value: 129 MPa Grade Count:4
Flexural Modulus 3.10 - 4.70 GPaAverage value: 4.07 GPa Grade Count:4
Secant Modulus, MD 1.02 - 3.50 GPaAverage value: 1.91 GPa Grade Count:5
Secant Modulus, TD 1.00 - 3.50 GPaAverage value: 1.86 GPa Grade Count:5
Izod Impact, Notched 0.500 - 0.900 J/cmAverage value: 0.630 J/cm Grade Count:6
Coefficient of Friction 0.200 - 0.500Average value: 0.365 Grade Count:3
Tear Strength Test 500 - 1300Average value: 690 Grade Count:4
Elmendorf Tear Strength MD 260 - 460 gAverage value: 367 g Grade Count:3
Elmendorf Tear Strength TD 300 - 440 gAverage value: 357 g Grade Count:3
Elmendorf Tear Strength, MD 2.02 - 30.2 g/micronAverage value: 14.3 g/micron Grade Count:6
Elmendorf Tear Strength, TD 0.525 - 28.9 g/micronAverage value: 14.1 g/micron Grade Count:6
Taber Abrasion, mg/1000 Cycles 1.20 - 2.20Average value: 1.65 Grade Count:4
Film Tensile Strength at Break, MD 37.0 - 317 MPaAverage value: 96.7 MPa Grade Count:16
Film Tensile Strength at Break, TD 44.0 - 195 MPaAverage value: 102 MPa Grade Count:7
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 4.70e+12 - 1.20e+13 ohm-cmAverage value: 8.35e+12 ohm-cm Grade Count:6
Surface Resistance 1.90e+15 - 2.70e+15 ohmAverage value: 2.10e+15 ohm Grade Count:7
Dielectric Constant 4.80 - 5.60Average value: 5.30 Grade Count:15
Dissipation Factor 0.180 - 0.220Average value: 0.213 Grade Count:15
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 - 130 µm/m-°CAverage value: 84.3 µm/m-°C Grade Count:22
 46.0 - 130 µm/m-°C
@Temperature 55.0 - 100 °C
Average value: 71.6 µm/m-°C Grade Count:11
Specific Heat Capacity 2.40 J/g-°CAverage value: 2.40 J/g-°C Grade Count:15
Thermal Conductivity 0.340 - 0.360 W/m-KAverage value: 0.341 W/m-K Grade Count:15
Melting Point 156 - 195 °CAverage value: 176 °C Grade Count:42
Crystallization Temperature 144 - 163 °CAverage value: 156 °C Grade Count:12
Deflection Temperature at 0.46 MPa (66 psi) 80.0 - 100 °CAverage value: 91.8 °C Grade Count:11
Vicat Softening Point 155 - 173 °CAverage value: 164 °C Grade Count:11
Glass Transition Temp, Tg 48.0 - 72.0 °CAverage value: 60.5 °C Grade Count:35
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.51 - 1.54Average value: 1.53 Grade Count:14
Haze 0.500 - 7.00 %Average value: 1.88 % Grade Count:21
Gloss 70.0 - 100 %Average value: 86.9 % Grade Count:18
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 190 - 220 °CAverage value: 208 °C Grade Count:8
Melt Temperature 240 - 250 °CAverage value: 243 °C Grade Count:10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Selar® RB 421 EVOH Barrier Resin
Multibase TPSiV® 3010-60A Thermoplastic Silicone Vulcanizate
Multibase TPSiV® 3010-50A Thermoplastic Silicone Vulcanizate
Multibase TPSiV® 3011-50A Thermoplastic Silicone Vulcanizate
Overview of materials for Polypropylene, Molded

O1890 / 77780

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.