MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Bamberger Polymers Bapolene® 3257U Polyethylene, Injection Molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Bapolene 3257U is a high density polyethylene resin that offers improved cycle times, superior modulus and impact resistance. It complies with US FDA 21CFR177.1520 and has a UV protection package.

Applications: Pallets, crates, and pails.

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers

Key Words: Fast Molding Cycle; Food Contact Acceptable; Good Impact Resistance; High Stiffness
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.963 g/ccASTM D-792
Melt Flow 10 g/10 minASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3820 psiASTM D-638
Flexural Modulus 1.30 GPaASTM D-790
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
processInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total 6280 High Density Polyethylene, Injection Molding Resin
Bamberger Polymers Bapolene® 3262 Polyethylene, Injection Grade
Dow DOWLEX™ IP-10262 High Density Polyethylene
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade
Dow UNIVAL™ DMDC-6143 NT 7 High Density Polyethylene Resin (HDPE)

PBP1115 / 82858

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.