MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chase Electronic Coatings HumiSeal® 600 Thinner
Categories: Fluid; Solvent

Material Notes: The viscosity of HumiSeal® coatings may be adjusted for application purposes, using a compatible thinner. HumiSeal® Thinners are blends of solvents formulated to maintain and preserve the original system benefits. This HumiSeal® Thinners complies with North American air quality regulations and the RoHS Directive 2011/65/EC.

Information provided by Chase Electronic Coatings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³
Volatile Organic Compounds (VOC) Content 969 g/l969 g/l
Vapor Pressure 0.00507 bar3.80 torr
 
Thermal PropertiesMetricEnglishComments
Boiling Point 141 °C286 °F
Flash Point 47.0 °C117 °FTCC
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 MonthDOM
 
Descriptive Properties
Colorclear
Relative Evaporating Rate0.37BuAc = 1
Vapor Density4.6 x density of air

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHAS946 / 239807

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.