MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Ascend Performance Materials Starflam® SF0067 Nylon 12, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Starflam SF0067 is a Halogen Free and Red Phosphorous Free Flame Retardant, Glass Fiber Reinforced, Polyamide 12 Injection Molding Resin.

Property data for dry as molded samples; natural color

Former Eurostar product. Eurostar has been acquired by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³DAM; ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 101 MPa14600 psiDAM; ISO 527-2
Elongation at Break 3.3 %3.3 %DAM; ISO 527-2
Flexural Strength 140 MPa20300 psiDAM; ISO 178
Flexural Modulus 7.80 GPa1130 ksiDAM; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1U
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 155 °C311 °FUnannealed; DAM; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 210 - 230 °C410 - 446 °FInjection
Middle Barrel Temperature 220 - 250 °C428 - 482 °FInjection
Front Barrel Temperature 220 - 250 °C428 - 482 °FInjection
Melt Temperature 220 - 260 °C428 - 500 °FInjection
Mold Temperature 60.0 - 90.0 °C140 - 194 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 4.00 hour4.00 hourInjection
Moisture Content 0.20 %0.20 %Injection
 
Descriptive Properties
AdditiveFlame Retarding Agent
 Release agent
Agency RatingsISO, 1043 PA12 GF30 FR(40)
AppearanceNatural Color
FeaturesBromine Free
 Flame Retardant
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEUROST6910 / 240050

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.