MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LATI Latan 3E71 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Polyoxymethylene (POM). Toughened. High viscosity. Good elongation and impact resistance

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/cc
Linear Mold Shrinkage, Flow 0.023 - 0.027 cm/cm
Linear Mold Shrinkage, Transverse 0.0235 - 0.0275 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 35.0 MPa
Elongation at Break >= 100 %
@Temperature 23.0 °C
 >= 100 %
@Temperature 60.0 °C
 >= 100 %
@Temperature 90.0 °C
Tensile Modulus 650 MPa
@Temperature 90.0 °C
 1100 MPa
@Temperature 60.0 °C
 1900 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched NB
Charpy Impact, Notched 12.0 kJ/m²
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 VA solution
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 70.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
Vicat Softening Point 125 °C
@Load 5.00 kg
 
Processing PropertiesOriginal ValueComments
Melt Temperature 175 - 200 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 80.0 - 90.0 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LATI Latan 9 POM
LATI Latiohm 73/23-10 CNT POM
LATI Latan 23UVE71 POM
LATI Latan 23UV POM
LATI Latan 2 POM

PLATH9755 / 177451

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.