MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

General Plastics LAST-A-FOAM® TF-5070-7 Polyurethane Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: TF 5070 Energy Absorption, Fire-retardant High-density: This flexible series is nearly identical to the TF6070 Series foams, with the addition of offering flame retardation. These durable, long-lasting foams are formulated to absorb significant energy while protecting payloads. These products offer excellent creep resistance under high static stress, and are available as polyurethane foam sheets and blocks. The TF5070 series has been used as a “spring-damper” for submarine launch tubes. In the construction industry, these flexible urethane foams serve as shock isolation. Other applications include serving as an impact-mitigation pad for shipping containers, and vibration-damper pads for mechanical equipment. These products are available as sheets, blocks and molded parts.

Advantages:

  • Extremely durable
  • Relatively unharmed by environmental factors
  • Absorbs significant energy while protecting payloads
Applications
  • Underground missile silos
  • Nuclear submarine launch tubes
  • Shock-isolation systems for earthquake-prone buildings
  • Shock mounts and pads for shipping delicate items
  • Vibration damper pads for mechanical equipment

Information provided by General Plastics Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.112 g/cc0.00405 lb/in³ASTM D3574
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength  0.0241 MPa
@Strain 10 %
3.50 psi
@Strain 10 %
ASTM D3574
 0.0414 MPa
@Strain 50 %
6.00 psi
@Strain 50 %
ASTM D3574
 
Descriptive Properties
Percent Compression0.04158°F, ASTM D3574

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
General Plastics LAST-A-FOAM® FR-3706 Polyurethane Foam
General Plastics LAST-A-FOAM® R-9320 Thermal Isolation Blocks
General Plastics LAST-A-FOAM® EF-4005 Polyurethane Foam
General Plastics LAST-A-FOAM® EF-4003 Polyurethane Foam
3M RPF-C (0.32 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass

PGENR075 / 186861

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.