MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
BASF Ultraform® W 2320 003 PRO AT POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Product Description: Ultraform® W2320 003 PRO AT is a very easy flowing and rapidly freezing injection molding POM grade. This grade was developed for the medical device market. This grade complies with US Pharmacopeia: Biological Reactivity Tests, USP Plastic Class VI (USP VI), ISO 10993-5: Biological Evaluation of Medical Devices Part 5: Test for Cytotoxicity, DMF: A Drug Master File (DMF) has been registered at FDA for Ultraform® PRO and Food Contact: Ultraform® PRO is in compliance with multiple regional food contact regulations, especially for Europe and United States. Typical applications include functional parts in medical devices.

Availability: North America

Features: Food Contact Acceptable; Good Flow

Use: Medical/Healthcare Applications

Agency Ratings: DMF; EC 1907/2006 (REACH); FDA Food Contact; ISO 10993 Part 5; USP Class VI

RoSH Compliance: RoSH Compliant

Processing Method: Injection Molding

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccISO 1183
Water Absorption 0.20 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 0.80 %ISO 62
Maximum Moisture Content 0.15
Linear Mold Shrinkage, Flow 0.020 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.021 cm/cmISO 294-4
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 9430 psiISO 527-2
Elongation at Break 24 %Nominal; ISO 527-2
Elongation at Yield 8.0 %ISO 527-2
Tensile Modulus 413000 psiISO 527-1
Izod Impact, Notched (ISO) 2.40 ft-lb/in²
@Temperature -30.0 °C
ISO 180
 2.40 ft-lb/in²
@Temperature 22.8 °C
ISO 180
Charpy Impact Unnotched 90.0 ft-lb/in²
@Temperature -30.0 °C
ISO 179
 90.0 ft-lb/in²
@Temperature 22.8 °C
ISO 179
Charpy Impact, Notched 1.90 ft-lb/in²
@Temperature -30.0 °C
ISO 179
 2.10 ft-lb/in²
@Temperature 22.8 °C
ISO 179
Tensile Creep Modulus, 1000 hours 196000 psiISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.8
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.0050
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 61.0 µin/in-°FISO 11359-2
Melting Point 331 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 212 °FUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Melt Temperature 374 - 446 °F
Mold Temperature 140 - 248 °F
Drying Temperature 176 - 230 °F
Dry Time 2.00 - 4.00 hour
Injection Pressure 508 - 1020 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASG2118 / 310811

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.