MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Alloy Wire International RW 80 Ni-Cr Resistance Wire
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Used in heating elements and control resistors because of its electrical properties and resistance to oxidation under temperature cycling and frequent switching. Also used in hot cutting operations, line bending, band heaters, bag sealers, etc.

Information provided by Alloywire International.

Key Words: Similar alloys are Nichrome 80, Nichrome 5, Brightray C, Gilphy 80, Tophet A, Nikrothal 80, Chromalloy 8-, Cronix, Chromel A
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.31 g/cc
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000108 ohm-cm
@Temperature 20.0 °C
 0.000109 ohm-cm
@Temperature 100 °C
Temperature resistance factor (F) =1.006
 0.000110 ohm-cm
@Temperature 200 °C
Temperature resistance factor (F) =1.015
 0.000111 ohm-cm
@Temperature 300 °C
Temperature resistance factor (F) =1.028
 0.000113 ohm-cm
@Temperature 400 °C
Temperature resistance factor (F) =1.045
 0.000114 ohm-cm
@Temperature 700 °C
Temperature resistance factor (F) =1.057
 0.000114 ohm-cm
@Temperature 800 °C
Temperature resistance factor (F) =1.051
 0.000114 ohm-cm
@Temperature 900 °C
Temperature resistance factor (F) =1.052
 0.000115 ohm-cm
@Temperature 1000 °C
Temperature resistance factor (F) =1.062
 0.000115 ohm-cm
@Temperature 600 °C
Temperature resistance factor (F) =1.068
 0.000115 ohm-cm
@Temperature 500 °C
Temperature resistance factor (F) =1.065
 0.000116 ohm-cm
@Temperature 1100 °C
Temperature resistance factor (F) =1.071
 0.000117 ohm-cm
@Temperature 1200 °C
Temperature resistance factor (F) =1.080
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.5 µm/m-°C
@Temperature 20.0 - 100 °C
Maximum Service Temperature, Air 300 °CHot Cutting or Line Bending
 1200 °CHeating Element
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 20 %
Nickel, Ni 80 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Goodfellow Nichrome®, Tophet A® Nickel 80 Chromium 20 Alloy
Nichrome 35-20 Medium Temperature Resistor Material
Nichrome 60-15 Medium Temperature Resistor Material
Nichrome 40-20 Medium Temperature Resistor Material
Nichrome 70-30 Medium Temperature Resistor Material

NAWIRE90 / 121063

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.