Product Description: LD 605BA is a general purpose LDPE grade, characterized by good stiffness and good toughness. It’s easy processable. Availability: Africa & Middle East and Europe Additive: - Antiblock: No
- Slip: No
- Thermal Stabilizer: No
Applications: - Compounding
- Food Packaging
- Houseware Articles
- Injection Molding
- Masterbatch Base Resin
- Rigid Medium Sized Molding
Information provided by ExxonMobil |