MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Scotchkote™ HB 850 Epoxy Floor Coating
Categories: Polymer; Thermoset; Epoxy

Material Notes: Scotchkote Epoxy Floor Coating HB 850 has been specifically developed as a 100% solids protection system for application to a wide rage of floor surfaces.

Product Features:

  • Combines good application characteristic with excellent chemical resistance
  • Designed for application by brush or roller
  • Suitable for use on most floor surfaces in conjunction with the appropriate primer

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³
Solids Content 100 %100 %
Thickness 203 microns8.00 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 15.7 MPa2280 psiASTM D638
Impact Test 3.95 J2.91 ft-lbASTM D2794
Abrasion 2020[mg] per 1000 cycles, 1 kg, CS17 Wheel; ASTM D4060
 
Processing PropertiesMetricEnglishComments
Cure Time 360 min6.00 hourTouch Dry
 1440 min24.0 hourHard Dry
 10100 min168 hourFull Cure
 
Descriptive Properties
AppearanceLight Gray, Mid Gray, Dark Gray, Stone, Red, Mid Green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35312 / 170059

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.