MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Sarlink® TPV X6135N Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV X6100 series are engineered materials designed for consumer, automotive, and industrial applications requiring superior Colorability and elastic performance. This product is a low hardness, low density, multi-purpose thermoplastic vulcanizate that does not require pre-drying and can be processed by injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Colorability; Good Flexibility; Good Flow; Good Processability; Low Hardness; Low Density; Low Specific Gravity; Resilient

Uses: Automotive Applications; Consumer Applications; Industrial Applications; Rubber Replacement; Soft Touch Applications

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc0.0318 lb/in³ISO 1183
Viscosity 195 cP
@Shear Rate 206 1/s,
Temperature 200 °C
195 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  32
@Time 5.00 sec
32
@Time 0.00139 hour
Extruded; ISO 868
 36
@Time 5.00 sec
36
@Time 0.00139 hour
Injection Molded; ISO 868
Tensile Strength at Break 2.30 MPa334 psiFlow; ISO 37
 2.70 MPa392 psiAcross Flow; ISO 37
Tensile Stress at Strain  0.800 MPa
@Strain 100 %
116 psi
@Strain 100 %
Across Flow; ISO 37
 1.10 MPa
@Strain 100 %
160 psi
@Strain 100 %
Flow; ISO 37
Elongation at Break 370 %370 %Flow; ISO 37
 560 %560 %Across Flow; ISO 37
Tear Strength 10.5 kN/m60.0 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set  23 %
@Temperature 22.8 °C,
Time 79200 sec
23 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 30 %
@Temperature 70.0 °C,
Time 79200 sec
30 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 43 %
@Temperature 125 °C,
Time 252000 sec
43 %
@Temperature 257 °F,
Time 70.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Processing Temperature 182 - 227 °C360 - 440 °F
Rear Barrel Temperature 138 - 160 °C280 - 320 °F
Middle Barrel Temperature 166 - 193 °C330 - 380 °F
Front Barrel Temperature 177 - 227 °C350 - 440 °F
Nozzle Temperature 182 - 227 °C360 - 440 °F
Mold Temperature 15.6 - 54.4 °C60.0 - 130 °F
Back Pressure 0.345 - 1.03 MPa50.0 - 150 psi
Screw Speed 25 - 75 rpm25 - 75 rpm
 
Descriptive Properties
AppearanceNatural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chengdu Polyster 4502 High Performance Grade TPV
Barlog Plastics KEBAFLEX E 50.1 TPE-V, Shore A50
Barlog Plastics KEBAFLEX E 45.1 TPE-V, Shore A45
Barlog Plastics KEBAFLEX E 40.1 TPE-V, Shore A40
Alliance Polymers Viprene™ P50A-22U-BLK Thermoplastic Vulcanizate Elastomer

PTEKNQ1213 / 237704

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.