MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Tra-Con Tra-Bond 546S05 Dual-Cure Acrylate
Categories: Polymer; Adhesive; Thermoset

Material Notes: TRA-BOND 546S05 is a dual cure (UV/heat) acrylate featuring excellent adhesion to glass. Ultimate Tg attained and shadowed areas cured with 15 minute exposure to 100-120°C.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccCured
Viscosity 5500 cP5500 cPMixed (cp #40, 2.5 rpm)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8686
Adhesive Bond Strength >= 6.89 MPa>= 1000 psiLap shear, adhesion to glass
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 85.0 °C185 °FUltimate Tg, 10°C/min; TMA
 
Processing PropertiesMetricEnglishComments
Cure Time 0.0833 - 0.167 min0.00139 - 0.00278 hourUV exposure
 
Descriptive Properties
Color Light RedUncured
 Transparent YellowCured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAC135 / 71063

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.