MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elkem (Bluestar Silicones) CAF® 520 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: CAF 520 is a one component silicone elastomer curing at Room Temperature:
  • Neutral
  • Self-adhesive
  • Thixotrope
  • Translucent, white
Applications: 520 is a fast-curing, ready-to-use silicone elastomer suitable for sealing and bonding. It cross-links at room temperature to give a flexible seal. CAF 520 is used for following applications:
  • Sealing and bonding of plastic materials.
  • Bonding of headlight.
  • Industrial maintenance.
  • Domestic appliances.
  • Electronics.
  • Solar panels.
Advantages: CAF 520 combines the advantages of:
  • Primer-less adhesion.
  • Odourless, it is particularly well accepted in the workstation environment.
  • High cure rate.
Its mechanical properties and good adhesion to many surfaces allow perfect assembly and full sealing between materials of different types as glass, metals, ceramics and plastics.

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/cc
Storage Temperature 2.00 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 15ISO 868
Tensile Strength 58.0 psiadhesion to Polycarbonate, 1 mm thick, 7 days curing, norm NM748, 100% Cohesive failure
 87.0 psiadhesion to Epoxy-PES paint, on stainless steel, 1 mm thick, 7 days curing, norm NM748, 100% Cohesive failure
 102 psiadhesion to glass, 1 mm thick, 7 days curing, norm NM748, 100% Cohesive failure
 102 psiadhesion to Alu AG3, 1 mm thick, 7 days curing, norm NM748, 100% Cohesive failure
 102 psiadhesion to Stainless Steel, 1 mm thick, 7 days curing, norm NM748, 100% Cohesive failure
 160 psi
Elongation at Break 500 %
100% Modulus 0.0435 ksi
@Strain 100 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -60.0 °C
 
Processing PropertiesOriginal ValueComments
Extrusion Rate 50.0 g/min3 mm, 3 bars, nom 495A
Cure Time 5.00 - 8.00 minSkin formation
 7.00 hour
@Thickness 2.00 mm
 24.0 hour
@Thickness 4.00 mm
Tack-Free Time 30.0 min
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceNon flowing paste
ColorTranslucent, white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
NuSil LSR-5805 Liquid Silicone Rubbers (LSR)
Lotte Advanced Materials Starex® WR-9120 ASA, Unreinforced
Dow Q3-3559 SEMIFLOWABLE TEXTILE ELASTOMER
Dow JCR 6115

PBLUST093 / 191069

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.