MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials HiDura™ D0MW BK0804 PA612
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Unreinforced

Material Notes: HiDura™ D0MW BK0804 is a weatherable, lubricated, low viscosity PA612 molding grade. It exhibits excellent flow and release making it suitable for injection molding of thin parts (e.g. cable ties). It exhibits low moisture absorption, good chemical resistance, dimensional stability, and weather resistance making it ideal for outdoor applications. PA612 offers a unique balance of thermal, mechanical, and physical properties.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³DAM; ISO 1183
Water Absorption 0.39 %
@Temperature 23.0 °C,
Time 86400 sec
0.39 %
@Temperature 73.4 °F,
Time 24.0 hour
DAM; ISO 62
Moisture Absorption at Equilibrium 1.3 %
@Temperature 23.0 °C
1.3 %
@Temperature 73.4 °F
DAM; ISO 62
Linear Mold Shrinkage, Flow 0.022 cm/cm
@Thickness 2.00 mm
0.022 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.021 cm/cm
@Thickness 2.00 mm
0.021 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 34.0 MPa4930 psi50% RH; ISO 527-2
 50.0 MPa7250 psiDAM; ISO 527-2
Tensile Strength, Yield 51.0 MPa7400 psi50% RH; ISO 527-2
 63.0 MPa9140 psiDAM; ISO 527-2
Elongation at Break 19 %19 %DAM; ISO 527-2
 47 %47 %50% RH; ISO 527-2
Elongation at Yield 9.6 %9.6 %DAM; ISO 527-2
 14 %14 %50% RH; ISO 527-2
Tensile Modulus 1.60 GPa232 ksi50% RH; ISO 527-2
 2.30 GPa334 ksiDAM; ISO 527-2
Flexural Strength 45.0 MPa6530 psi50% RH; ISO 178
 71.0 MPa10300 psiDAM; ISO 178
Flexural Modulus 1.70 GPa247 ksi50% RH; ISO 178
 2.40 GPa348 ksiDAM; ISO 178
Izod Impact, Notched (ISO)  4.00 kJ/m²
@Temperature -40.0 °C
1.90 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 4.30 kJ/m²
@Temperature -30.0 °C
2.05 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 4.90 kJ/m²
@Temperature 23.0 °C
2.33 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 5.50 kJ/m²
@Temperature -40.0 °C
2.62 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 180/1A
 5.60 kJ/m²
@Temperature -30.0 °C
2.66 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 8.60 kJ/m²
@Temperature 23.0 °C
4.09 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DAM; ISO 179/1eU
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.340 J/cm²
@Temperature -40.0 °C
1.62 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 0.350 J/cm²
@Temperature -30.0 °C
1.67 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.470 J/cm²
@Temperature -40.0 °C
2.24 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 179/1eA
 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 0.590 J/cm²
@Temperature -30.0 °C
2.81 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 38.0 kV/mm
@Thickness 1.00 mm
965 kV/in
@Thickness 0.0394 in
DAM; IEC 60243
 
Thermal PropertiesMetricEnglishComments
Melting Point 218 °C424 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 154 °C309 °FUnannealed; 50% RH; ISO 75-2/B
 155 °C311 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FUnannealed; DAM; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Melt Temperature >= 235 °C>= 455 °FInjection
 <= 290 °C<= 554 °FInjection
Mold Temperature >= 50.0 °C>= 122 °FInjection
 <= 90.0 °C<= 194 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time >= 4.00 hour>= 4.00 hourInjection
 <= 6.00 hour<= 6.00 hourInjection
Moisture Content 0.15 %0.15 %Injection
 
Descriptive Properties
AdditiveLubricant
AppearanceBlack
FeaturesAbrasion Resistance
 Chemical Resistant
 Excellent Processability
 Fast Molding Cycle
 Good Dimensional Stability
 Good Flow
 Good Mold Release
 High Flow
 Low Viscosity
 Lubricated
 Weatherable
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE9002 / 287543

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.