MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Silberline Sparkle Silver® 3000-AR
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Sparkle Silver® 3000-AR is a medium, high sparkle, brilliant, non-leafing aluminum pigment popular for solvent Automotive Applications. It shows exceptional resistance to spotting when incorporated into paint finishes that are subjected to a variety of environmental conditions such as; industrial fumes, tree sap, and bird droppings. This pigment can be used with tints to produce a wide range of polychromatic effects.

Applications: Automotive

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.47 g/cc
Bulk Factor 0.081
Volatiles 35 %
Particle Size 28 µm
Particle Mesh Size <= 325 Mesh2% retained
 
Descriptive Properties
SolventsMineral Spirits/High Flash

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Molybdenum Disilicide, MoSi2
Nickel silver 65-10, UNS C74500, OSO70 Temper flat products
Oxygen-free silver-bearing Copper, UNS C10400, H00 Temper flat products
Silver-Copper Eutectic Alloy (72Ag-28Cu; UNS P07720; AWS BAg-8), Cold Drawn then Annealed at 250°C (480°F)
Silver-Magnesium-Nickel Alloy Strip (Ag-0.25Ni-0.25Mg), Soft Temper

ESIBER001 / 5756

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.