Georgia Gulf 7765 is a general-purpose indoor rigid PVC profile extrusion compound designed for applications requiring the following properties. 7765 carries an NSF standard 51 listing (for food zone). - Impact Strength & Toughness
- Flame Retardant
- Colorability
- Dimensional Stability
- Chemical Resistance
- Stiffness(High Modulus)
Information provided by Georgia Gulf Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued. |