MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M 9475LE High Strength Double Coated Tape with Adhesive 300LSE
Categories: Polymer; Adhesive

Material Notes: 3M™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acrylic adhesive also provides excellent adhesion to surfaces contaminated lightly with oil typically used with machine parts.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 0.500 milCarrier
 2.00 milFaceside Adhesive
 2.00 milBackside Adhesive
 4.50 milTotal Thickness
 6.20 milCaliper
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 2.8125 pliStainless Steel, 180° peel, 2 mil Al foil backing, 15 min RT, Faceside; ASTM D3330
 3.75 pliGlass, 90° peel, 2 mil Al foil backing, 72 hr RT, Faceside; ASTM D3330
 3.75 pliPolypropylene, 90° peel, 2 mil Al foil backing, 72 hr RT, Faceside; ASTM D3330
 4.375 pliStainless Steel, 180° peel, 2 mil Al foil backing, 72 hr RT, Faceside; ASTM D3330
 4.375 pliPolypropylene, 90° peel, 2 mil Al foil backing, 72 hr RT, Backside; ASTM D3330
 4.375 pliStainless Steel, 180°, 2 mil polyester as backing, 72 hr RT, Faceside; ASTM D3330
 4.375 pliStainless Steel, 180° peel, 2 mil Al foil backing, 15 min RT, Backside; ASTM D3330
 4.6875 pliGlass, 90° peel, 2 mil Al foil backing, 72 hr RT, Backside; ASTM D3330
 5.00 pliStainless Steel, 180°, 2 mil polyester as backing, 72 hr RT, Backside; ASTM D3330
 5.3125 pliABS, 90° peel, 2 mil Al foil backing, 72 hr RT, Faceside; ASTM D3330
 5.625 pliStainless Steel, 180° peel, 2 mil Al foil backing, 72 hr RT, Backside; ASTM D3330
 5.625 pliStainless Steel, 180° peel, 2 mil Al foil backing, 72 hr 70°C, Faceside; ASTM D3330
 5.625 pliABS, 90° peel, 2 mil Al foil backing, 72 hr RT, Backside; ASTM D3330
 6.5625 pliStainless Steel, 180° peel, 2 mil Al foil backing, 72 hr 70°C, Backside; ASTM D3330
 7.50 pliPolycarbonate, 90° peel, 2 mil Al foil backing, 72 hr RT, Faceside; ASTM D3330
 7.50 pliPolycarbonate, 90° peel, 2 mil Al foil backing, 72 hr RT, Backside; ASTM D3330
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 93.0 °CLong term
 149 °CShort term
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
Liner#83 Polycoated Kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM33275 / 168022

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.