MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Resin Technology Group DP031199-1 Cationic UV Cure Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: DP031199-1 is an epoxy-based, low-viscosity, cationic-curable adhesive/sealant. This product is activated by exposure to medium intensity UV radiation resulting in a strong, chemically resistant, low out-gassing polymer system. This UV curable adhesive is soft and flexible and cures tack free.

Developmental Product:

This data was generated on laboratory material and should not be used for specification purposes. The Developmental Product name and designation may change upon commercialization.

Processing:

UV light cure: Intensity of 200 mw/cm2; Spectral output of 300 to 500 nanometers; Optimum wavelength of 375 nanometers

Recommended Aurora UV light sources:

  • Aurora 455-S 5x5 High Intensity Flood
  • Aurora 461-S 1x6 High Intensity Beam
  • Aurora 100-S Spot Light Guide

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/ccUncured
Viscosity 1500 cP
@Temperature 25.0 °C
1500 cP
@Temperature 77.0 °F
Uncured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050Cured
Elongation at Break 8.0 %8.0 %Cured
Shear Strength 41.4 MPa6000 psiCured, tensile
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 160 °C320 °FCured
Minimum Service Temperature, Air -50.0 °C-58.0 °FCured
Flash Point >= 93.3 °C>= 200 °FUncured
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 80 %80 %Mfr. Specifies clear but does not quantify
 
Descriptive Properties
ColorClear
CompositionEpoxy
Moisture ResistanceExcellentCured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Monprene® MP-1875UV Thermoplastic Elastomer
RTP Company RTP 2800 B-55A Thermoplastic Polyolefin Elastomer (TEO)
RTP Company RTP 2800 B-45A FR A UV Thermoplastic Polyolefin Elastomer (TEO) Flame Retardant - PBDE Free - UV Stabilized
Resinlab® RC8080 Anaerobic Retaining Compound
Resinlab® RC8020 Anaerobic Retaining Compound

PRESINT652 / 65536

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.