MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger Sintimid™ ESD 23 Polyamide-imide (PAI)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI)

Material Notes: SINTIMID™ ESD 23 has the highest compressive strength and use temperature of the group. It is based on an Ensinger-Hyde manufactured polyamide-imide resin with a low sloughing, additive package.

Information Provided by Ensinger Industries, Inc.
Sintimid has been replaced with Tecasint in the Ensinger product line.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.42 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 93ASTM D2240
Tensile Strength, Yield 12300 psiASTM D638
Elongation at Break 2.7 %ASTM D638
Tensile Modulus 580000 psiASTM D638
Flexural Strength 19500 psiASTM D790
Compressive Strength 34800 psiASTM D695
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+8 - 1.00e+11 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear 22.5 µin/in-°F
Maximum Service Temperature, Air 595 °Fcontinuous
Deflection Temperature at 1.8 MPa (264 psi) 600 °FASTM D648
Flammability, UL94 V-0
 
Descriptive Properties
Base MaterialPAI

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyamide-Imide, Molded
Hippe PAI Polyamide-imide
Mitsubishi Chemical Advanced Materials Duratron™ T4203 PAI Extruded Polyamide-imide
Mitsubishi Chemical Advanced Materials Semitron™ ESd 520HR PTFE
Overview of materials for Polyamide-Imide, Glass Filled

PENSIN006 / 92823

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.