MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI Type S15500 (15Cr-5Ni) Precipitation Hardening Stainless Steel transverse direction, condition H900
Categories: Metal; Ferrous Metal; Stainless Steel; Precipitation Hardening Stainless; T S10000 Series Stainless Steel

Material Notes: Martensitic, precipitative hardening (maraging), combining high strength and hardness with excellent corrosion resistance. Applications include valve parts, fittings and fasteners, shafts, gears, chemical process equipment, paper mill equipment, aircraft components and nuclear reactor components.

Property data taken from intermediate location on sample.

Key Words: 15-5 PH, 15-5PH, 15/5 PH, 15/5PH, XM12, AMS 5862, ASME SA705 (XM-12), ASTM A564 (XM-12), ASTM A693 (XM-12), ASTM A705 (XM-12), AFNOR NF A35-581 Z6CNU15.05, DIN 1.4540, DIN X4CrNiCuNb164, Cr-Ni 15-5, UNS S15500, AMS 5658, AMS 5659, AMS 5826
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.80 g/ccSolution treated plus 480°C for 1 hour, air cooled.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 420
Hardness, Knoop 451Converted from Brinell
Hardness, Rockwell B 104Converted from Brinell
Hardness, Rockwell C 44.2Converted from Brinell
Hardness, Vickers 445Converted from Brinell
Tensile Strength, Ultimate 1380 MPa
Tensile Strength, Yield 1275 MPa
@Strain 0.2 %
Elongation at Break 10 %in 50 mm
Modulus of Elasticity 200 GPaTypical elastic modulus for stainless steel
Charpy Impact 10.0 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000770 ohm-cmSolution treated plus 480°C for 1 hour, air cooled.
Magnetic Permeability 95approximate value for the annealed condition at RT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.4 µm/m-°C
@Temperature -73.0 - 21.0 °C
 10.8 µm/m-°C
@Temperature 21.0 - 205 °C
 10.8 µm/m-°C
@Temperature 21.0 - 93.0 °C
 11.3 µm/m-°C
@Temperature 21.0 - 315 °C
Specific Heat Capacity 0.420 J/g-°CSolution treated plus 480°C for 1 hour, air cooled.
Thermal Conductivity 17.8 W/m-K
@Temperature 150 °C
 19.5 W/m-K
@Temperature 260 °C
 22.5 W/m-K
@Temperature 460 °C
 22.7 W/m-K
@Temperature 480 °C
Melting Point 1405 - 1440 °C
Solidus 1405 °C
Liquidus 1440 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.070 %
Chromium, Cr 14.8 %
Copper, Cu 3.5 %
Iron, Fe 75 %
Manganese, Mn <= 1.0 %
Nb + Ta 0.30 %
Nickel, Ni 4.5 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type S15500 (15Cr-5Ni) Precipitation Hardening Stainless Steel transverse direction, condition H925
AISI Type S15500 (15Cr-5Ni) Precipitation Hardening Stainless Steel transverse direction, condition H1025
AISI Type S15500 (15Cr-5Ni) Precipitation Hardening Stainless Steel longitudinal direction, condition H900
17-7 PH Stainless Steel, CH900, plate, sheet, and strip
AISI Type S15500 (15Cr-5Ni) Precipitation Hardening Stainless Steel, condition H925

MQM15AA / 13513

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.