MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Resinlab® EP1320LV Heat Cure Epoxy Conformal Coating
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the application requires low shrinkage and excellent adhesion to a wide variety of plastics, metals and circuit board materials. These products give very good environmental protection and dielectric properties over a wide temperature range. The primary difference between the two versions is the LV version has a lower high shear viscosity (higher press flow rate) to provide easier dispensing. The amount of sag upon curing is the same.

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/ccTM R050-16
Water Absorption 0.13 %
@Time 86400 sec
0.13 %
@Time 24.0 hour
TM R050-35
Viscosity 36400 cP
@Shear Rate 1.00 1/s
36400 cP
@Shear Rate 1.00 1/s
Mixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585
Tensile Strength at Break 10.3 MPa1500 psiTM R050-36
Tensile Strength, Ultimate 10.3 MPa1500 psiTM R050-36
Tensile Strength, Yield 2.76 MPa400 psiTM R050-36
Elongation at Break 10 - 15 %10 - 15 %TM R050-36
Tensile Modulus 0.345 - 0.483 GPa50.0 - 70.0 ksiTM R050-36
Compressive Yield Strength 89.6 MPa13000 psiTM R050-38
Compressive Strength 110 MPa16000 psiBreak; TM R050-38
 124 MPa18000 psiUltimate; TM R050-38
Compressive Modulus 4.14 GPa600 ksiTM R050-38
Adhesive Bond Strength 11.7 MPa1700 psiLap Shear-Aluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+16 ohm-cm2.00e+16 ohm-cm
Dielectric Constant  3.2
@Frequency 100000 Hz
3.2
@Frequency 100000 Hz
 3.4
@Frequency 100 Hz
3.4
@Frequency 100 Hz
Dielectric Strength 17.3 kV/mm440 kV/in
Dissipation Factor  0.020
@Frequency 100 Hz
0.020
@Frequency 100 Hz
 0.020
@Frequency 100000 Hz
0.020
@Frequency 100000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear  59.0 µm/m-°C
@Temperature <=86.0 °C
32.8 µin/in-°F
@Temperature <=187 °F
Below Tg
 205 µm/m-°C
@Temperature >=86.0 °C
114 µin/in-°F
@Temperature >=187 °F
Above Tg
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Glass Transition Temp, Tg 86.0 °C187 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  5.00 - 10.0 min
@Temperature 150 °C
0.0833 - 0.167 hour
@Temperature 302 °F
 15.0 min
@Temperature 120 °C
0.250 hour
@Temperature 248 °F
 30.0 min
@Temperature 110 °C
0.500 hour
@Temperature 230 °F
 
Descriptive Properties
Appearanceblack liquid
Mix Ratio by Volumeone part
Side-By-Side Cartridges CapableNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Resinlab® EP1320 Heat Cure Epoxy Conformal Coating
Overview of materials for Phenolic, Ablative Coating
Master Bond EP31 High Shear and Peel Strength Room Temperature Curing Epoxy
Master Bond EP21ANHT Two Component, Room Temperature Curing Epoxy Adhesive
Master Bond EP17HT-LO One component epoxy system for bonding, sealing, coating and casting

PRESL139 / 101553

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.