MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman PP 1407L-01 Polypropylene High-Impact Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Description

Polypropylene PP 1407L-01 is a super high-impact copolymer polypropylene.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D792
Melt Flow 1.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7575ASTM D785
Tensile Strength, Yield 25.0 MPa3630 psi50 mm/min; ASTM D638
Elongation at Yield 10 %10 %ASTM D638
Flexural Modulus 1.00 GPa145 ksi5 mm/min, secant; ASTM D790
Izod Impact, Notched NBNBASTM D256
Izod Impact, Unnotched NBNBASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C180 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman POLYFORT™ FPP 1239H Glass Filled Chemically Coupled Homopolymer Polypropylene
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer
A. Schulman TPP20AF20BK 20% Talc-Filled, Heat-Stabilized, Homopolymer Propylene containing 25% P.C.R.
Flint Hills P6E2A-005 Impact Copolymer Polypropylene
Formosa Plastics Formolene® 2302E Impact Copolymer Polypropylene

PASHU221 / 25185

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.