MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Trinseo STYRON™ 6500 Ignition Resistant Polystyrene Resin
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: STYRON™ 6500 is an ignition-resistant polystyrene resin with excellent balance of strength, heat resistance and flow properties that are tailor-made for consumer electronics applications. It is a non-deco ignition resistant polystyrene which is free from polybrominated diphenyl ether (PBDPE) and polybrominated biphenyl (PBB). It is designed for injection molding application.

Main Characteristics:

  • Good flow
  • Excellent het resistance
  • UL 94 V-0 @ 1.5 mm
Applications:
  • LCD TV

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 in/in
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 13.8 MPaCompression Molded; ASTM D638
 19.3 MPaInjection Molded; ASTM D638
Tensile Strength, Yield 17.2 MPaCompression Molded; ASTM D638
 20.7 MPaInjection Molded; ASTM D638
Elongation at Break 30 %Compression Molded; ASTM D638
 40 %Injection Molded; ASTM D638
Flexural Strength 33.8 MPaCompression Molded; ASTM D790
 40.7 MPaInjection Molded; ASTM D790
Flexural Modulus 1990 MPaCompression Molded; ASTM D790
 2370 MPaInjection Molded; ASTM D790
Izod Impact, Notched 64.0 J/m
@Temperature 23.0 °C
Compression Molded; ASTM D256
 80.0 J/m
@Temperature 23.0 °C
Injection Molded; ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 76.0 µm/m-°CASTM D696
Vicat Softening Point 100 °CASTM D1525
Flammability, UL94 V-0
@Thickness 1.50 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total Lacqrene® 4241 High Impact Polystyrene
Chi Mei Polyrex® PH-888H Polystyrene - High Impact
Americas Styrenics STYRON® 478 High Impact Polystyrene
Americas Styrenics STYRON® 649D High Heat Crystal Polystyrene
Americas Styrenics STYRON™ 487 High-Impact Polystyrene Resin

PDWST090 / 142299

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.