MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sciengy AS-SG401E87 PPS/PA66, Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler

Material Notes: AS-SG401E87 is a glass fiber reinforced by PPS based PA66 alloy to provide excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low flash characteristics, and fast cycle times. It may be easily molded in conventional injection molding equipment utilizing water heated molds

Information provided by Shandong Sciengy New Materials Co. Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.55 g/ccISO 1183
Water Absorption at Saturation 0.20 %ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cmGB/T 15585
Linear Mold Shrinkage, Transverse 0.0080 cm/cmGB/T 15585
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 180 MPaISO 527
Elongation at Break 2.0 %ISO 527
Flexural Strength 260 MPaISO 178
Flexural Modulus 12.0 GPaISO 178
Charpy Impact, Notched 8.00 kJ/m²IS0 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 4.0IEC 60250
Dielectric Strength 22.0 kV/mmIEC 60243
Dissipation Factor 0.0030IEC 60250
Comparative Tracking Index 250 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 280 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 250 °CISO 75
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Melt Temperature 290 - 330 °CInjection molding; ISO 294
Mold Temperature 120 - 160 °CInjection molding; ISO 294
Drying Temperature 150 °C
@Time 10800 sec
Injection Pressure 30.0 - 100 MPa
 
Descriptive Properties
Limit in-cylinder retention time300?/60min
 320?/30min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSCIE041 / 297088

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.