Availability: Asia Pacific; Europe; North America Fillers/Reinforcement: Glass Fiber, 25% Filler by Weight Additive: Heat Stabilizer; Lubricant Features: Good Dimensional Stability; Good Impact Resistance; Heat Stabilized; Lubricated Form: Pellets Processing Method: Injection Molding Information provided by Teknor Apex |