Physical Properties | Metric | English | Comments |
---|
Density | 1.0574 g/cc @Temperature 100 °C | 0.038201 lb/in³ @Temperature 212 °F |
| 1.1087 g/cc @Temperature -5.00 °C | 0.040054 lb/in³ @Temperature 23.0 °F |
| 1.888 g/cc @Temperature 40.0 °C | 0.06821 lb/in³ @Temperature 104 °F |
Viscosity | 0.45 cP @Temperature 100 °C | 0.45 cP @Temperature 212 °F |
| 0.56 cP @Temperature 80.0 °C | 0.56 cP @Temperature 176 °F |
| 0.72 cP @Temperature 60.0 °C | 0.72 cP @Temperature 140 °F |
| 0.98 cP @Temperature 40.0 °C | 0.98 cP @Temperature 104 °F |
| 1.39 cP @Temperature 20.0 °C | 1.39 cP @Temperature 68.0 °F |
| 1.71 cP @Temperature 10.0 °C | 1.71 cP @Temperature 50.0 °F |
| 2.13 cP @Temperature 0.000 °C | 2.13 cP @Temperature 32.0 °F |
| 2.73 cP @Temperature -10.0 °C | 2.73 cP @Temperature 14.0 °F |
Molecular Weight | 36.47 g/mol | 36.47 g/mol |
Vapor Pressure | 0.00200 bar @Temperature -10.0 °C | 1.50 torr @Temperature 14.0 °F |
| 0.00300 bar @Temperature 0.000 °C | 2.25 torr @Temperature 32.0 °F |
| 0.00700 bar @Temperature 10.0 °C | 5.25 torr @Temperature 50.0 °F |
| 0.0140 bar @Temperature 20.0 °C | 10.5 torr @Temperature 68.0 °F |
| 0.0460 bar @Temperature 40.0 °C | 34.5 torr @Temperature 104 °F |
| 0.130 bar @Temperature 60.0 °C | 97.5 torr @Temperature 140 °F |
| 0.330 bar @Temperature 80.0 °C | 248 torr @Temperature 176 °F |
| 0.750 bar @Temperature 100 °C | 563 torr @Temperature 212 °F |
Surface Tension | 0.064 dynes/cm @Temperature 100 °C | 0.064 dynes/cm @Temperature 212 °F |
| 0.067 dynes/cm @Temperature 80.0 °C | 0.067 dynes/cm @Temperature 176 °F |
| 0.068 dynes/cm @Temperature 60.0 °C | 0.068 dynes/cm @Temperature 140 °F |
| 0.070 dynes/cm @Temperature 40.0 °C | 0.070 dynes/cm @Temperature 104 °F |
| 0.072 dynes/cm @Temperature 10.0 °C | 0.072 dynes/cm @Temperature 50.0 °F |
| 0.072 dynes/cm @Temperature 20.0 °C | 0.072 dynes/cm @Temperature 68.0 °F |
| 0.073 dynes/cm @Temperature 0.000 °C | 0.073 dynes/cm @Temperature 32.0 °F |
| 0.074 dynes/cm @Temperature -10.0 °C | 0.074 dynes/cm @Temperature 14.0 °F |
|
Thermal Properties | Metric | English | Comments |
---|
Specific Heat Capacity | 2.80 J/g-°C @Temperature -10.0 °C | 0.669 BTU/lb-°F @Temperature 14.0 °F |
| 2.80 J/g-°C @Temperature 0.000 °C | 0.669 BTU/lb-°F @Temperature 32.0 °F |
| 2.90 J/g-°C @Temperature 10.0 °C | 0.693 BTU/lb-°F @Temperature 50.0 °F |
| 2.90 J/g-°C @Temperature 20.0 °C | 0.693 BTU/lb-°F @Temperature 68.0 °F |
| 3.00 J/g-°C @Temperature 40.0 °C | 0.717 BTU/lb-°F @Temperature 104 °F |
| 3.10 J/g-°C @Temperature 60.0 °C | 0.741 BTU/lb-°F @Temperature 140 °F |
| 3.20 J/g-°C @Temperature 80.0 °C | 0.765 BTU/lb-°F @Temperature 176 °F |
| 3.30 J/g-°C @Temperature 100 °C | 0.789 BTU/lb-°F @Temperature 212 °F |
Thermal Conductivity | 0.480 W/m-K @Temperature -10.0 °C | 3.33 BTU-in/hr-ft²-°F @Temperature 14.0 °F |
| 0.490 W/m-K @Temperature 0.000 °C | 3.40 BTU-in/hr-ft²-°F @Temperature 32.0 °F |
| 0.500 W/m-K @Temperature 10.0 °C | 3.47 BTU-in/hr-ft²-°F @Temperature 50.0 °F |
| 0.510 W/m-K @Temperature 20.0 °C | 3.54 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
| 0.530 W/m-K @Temperature 40.0 °C | 3.68 BTU-in/hr-ft²-°F @Temperature 104 °F |
| 0.550 W/m-K @Temperature 60.0 °C | 3.82 BTU-in/hr-ft²-°F @Temperature 140 °F |
| 0.570 W/m-K @Temperature 80.0 °C | 3.96 BTU-in/hr-ft²-°F @Temperature 176 °F |
| 0.590 W/m-K @Temperature 100 °C | 4.09 BTU-in/hr-ft²-°F @Temperature 212 °F |
Melting Point | -60.0 °C | -76.0 °F |
Boiling Point | 109 °C @Pressure 0.101 MPa | 228 °F @Pressure 14.6 psi |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view