MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow ATTANE™ 4401 Ultra Low Density Polyethylene, Blown Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Very Low Density Polyethylene (VLDPE)

Material Notes: ATTANE® 4401 copolymer is an ultra low density polyethylene having high tear strength and impact resistance. It is designed for use in industrial/consumer film applications, either as high performance monolayer blown film or as part of a multilayer film as well as for use in molded durable applications requiring high strength, flexibility, and environmental stress crack resistance. ATTANE 4401 is an excellent resin for blending. It complies with FDA regulation 21 CFR 177.1520 (c) 3.2a for food contact.

Film properties below based on a film thickness of 38 µm. Data provided by Dow Chemical.

Key Words: ULDPE, VLDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.912 g/cc
Thickness 38.0 microns
Melt Flow 1.0 g/10 min
@Load 2.16 kg
Melt flow ratio I10/I2 is 8.7.
 
Mechanical PropertiesOriginal ValueComments
Elmendorf Tear Strength MD 650 g
Elmendorf Tear Strength TD 826 g
Elmendorf Tear Strength, MD 17.1 g/micron
Elmendorf Tear Strength, TD 21.7 g/micron
Dart Drop >= 21.8 g/micron
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 95.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 96.0 °CSeal initiation temperature
 225 °CFilm extrusion temperature
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow ATTANE™ 4501 Ultra Low Density Polyethylene, Blown Film Grade
Dow ATTANE™ 4402 Ultra Low Density Polyethylene, Cast Film Grade
Dow ATTANE™ 4403 Ultra Low Density Polyethylene, Blown Film Grade
DuPont 20 Series 20-6064 Specialty Polyethylene Resin
Dow ATTANE™ 4202 Ultra Low Density Polyethylene, Cast Film Grade

PDW418 / 34487

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.